Optical constants of HIKARI - F (Flint)
F2
Wavelength:
µm
(0.320 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.545002-0.001337396λ^{2}+0.02801151λ^{-2}-0.0005417021λ^{-4}+0.0001501754λ^{-6}-3.617071\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.620040 Vd: 36.331342 glass_code: 620363 glass_status: preferred density: 3.61 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.6e-06 K-1
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links