Optical constants of HIKARI - F (Flint)
E-F8
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.47286461-0.00151192688λ^{2}+0.0276004612λ^{-2}-0.00152550371λ^{-4}+0.000290711488λ^{-6}-1.28484326\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.595510 Vd: 39.216011 glass_status: preferred density: 2.63 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.4e-06 K-1 dPgF: -0.0009
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon