Optical constants of HIKARI - F (Flint)
E-F2
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.55739282-0.0107951229λ^{2}+0.0216807328λ^{-2}+0.00105165979λ^{-4}-5.36309816\text{×}10^{-05}λ^{-6}+7.7466326\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.620041 Vd: 36.258932 glass_code: 620363 glass_status: preferred density: 2.69 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.9e-06 K-1 dPgF: 0.0045
Comments
Melt Freq: 1
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon