Optical constants of HIKARI - F (Flint)
E-F16
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.47196413-0.0100810083λ^{2}+0.0208698749λ^{-2}+0.000995620952λ^{-4}-4.77932855\text{×}10^{-05}λ^{-6}+8.07129922\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.592701 Vd: 35.298957 glass_status: preferred density: 2.64 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.8e-06 K-1 dPgF: 0.0079
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon