Optical constants of HIKARI - F (Flint)
E-F1
Wavelength:
µm
(0.4 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.56251919-0.00314623487λ^{2}+0.0291600242λ^{-2}-0.000870730012λ^{-4}+0.000226533195λ^{-6}-8.61239946\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.625882 Vd: 35.649694 glass_status: preferred density: 2.72 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.3e-06 K-1 dPgF: 0.0006
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon