Optical constants of HIKARI - BaSF (Barium dense flint)
E-BASF6

Wavelength: µm
 (0.4 – 0.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.71377616-0.00941072521λ^{2}+0.0221914885λ^{-2}+0.000735180213λ^{-4}-2.11522864\text{×}10^{-05}λ^{-6}+3.73099495\text{×}10^{-06}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 23.0 ℃
nd: 1.667551
Vd: 41.964323
glass_status: preferred
density: 3.2 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 8e-06 K-1
dPgF: 0.0003

References

NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Hikari Glass Co., Ltd.

Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.

External links


Glass

External links