Optical constants of HIKARI - BaSF (Barium dense flint)
BASF8
Wavelength:
µm
(0.360 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.881495-0.006454381λ^{2}+0.03074684λ^{-2}-0.0001396031λ^{-4}+0.0001314241λ^{-6}-2.44494\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.723421 Vd: 37.969147 glass_code: 723380 glass_status: preferred density: 3.79 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9e-06 K-1 dPgF: 0.0039
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets