Optical constants of HIKARI - BaK (Barium crown)
E-BAK1
Wavelength:
µm
(0.290 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.44353274-0.0161455184λ^{2}+0.00881927898λ^{-2}+0.00144687542λ^{-4}-0.000136331798λ^{-6}+6.03309808\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.572500 Vd: 57.738955 glass_code: 572577 glass_status: preferred density: 3.16 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.5e-06 K-1 dPgF: 0.0003
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
BAK1 optical glass
BAK1 is a very popular optical glass. Most glass makers produce this or very similar glass.BAK1 or similar glasses produced by different makers
Maker | Glass |
---|---|
Schott | N-BAK1 |
Hikari | E-BAK1 |
Ohara | S-BAL11 |
CDGM | H-BAK8 |
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon