Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.319725+0.002602493λ^{2}+0.02249807λ^{-2}-0.002672041λ^{-4}+0.0003926686λ^{-6}-2.043303\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.539960 Vd: 59.681919 glass_code: 540597 glass_status: preferred density: 2.85 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.7e-06 K-1 dPgF: 0.0021
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon