Optical constants of HIKARI - BaF (Barium flint)
J-BAF12
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.62810335-0.00995087731λ^{2}-0.000144740792λ^{4}+0.0206473464λ^{-2}+0.000162531777λ^{-4}+7.85240289\text{×}10^{-05}λ^{-6}-7.45350927\text{×}10^{-06}λ^{-8}+4.83617341\text{×}10^{-07}λ^{-10}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.86e-06 1.3085e-08 -2.2674e-12 7.946e-07 9.6385e-10 0.17031 nd: 1.639300 Vd: 44.834133 density: 3.23 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.7e-06 K-1 dPgF: 0.0005 phosphate_resistance: 2.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon