Optical constants of HIKARI - BaF (Barium flint)
E-BAF8

Wavelength: µm
 (0.350 – 0.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.58072694-0.00826682499λ^{2}+0.0192773695λ^{-2}+0.000287391647λ^{-4}+1.54399962\text{×}10^{-05}λ^{-6}+4.63747358\text{×}10^{-07}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 23.0 °C
nd: 1.623740
Vd: 47.044346
glass_code: 624470
glass_status: preferred
density: 3.14 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 8e-06 K-1
dPgF: -0.0031

References

NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Hikari Glass Co., Ltd.

Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.