Optical constants of HIKARI - BaF (Barium flint)
E-BAF12
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.62833748-0.0100974072λ^{2}+0.0203176439λ^{-2}+0.000375302287λ^{-4}+1.45983254\text{×}10^{-05}λ^{-6}+1.37126433\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.639300 Vd: 44.882939 glass_code: 639449 glass_status: preferred density: 3.22 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8e-06 K-1 dPgF: -0.0007
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon