Optical constants of HIKARI - BaF (Barium flint)
E-BAF10
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.72932262-0.0106085219λ^{2}+0.0204478583λ^{-2}+0.000484576944λ^{-4}-3.06411426\text{×}10^{-06}λ^{-6}+1.63981487\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.670029 Vd: 47.236541 glass_code: 670472 glass_status: preferred density: 3.82 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.3e-06 K-1 dPgF: -0.0022
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets