Optical constants of HIKARI - BaF (Barium flint)
BAF10
Wavelength:
µm
(0.350 – 0.7)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.708194+0.004899893λ^{2}+0.03147874λ^{-2}-0.002304342λ^{-4}+0.0003414449λ^{-6}-1.465281\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.670030 Vd: 47.049915 glass_code: 670471 glass_status: preferred density: 3.83 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.5e-06 K-1 dPgF: -0.0008
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon