Optical constants of CDGM - ZPK (Dense phosphate crown)
D-ZPK1A-25
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.860621496λ^2}{λ^2-0.0142471941}+\frac{0.723408663λ^2}{λ^2-0.00293226364}+\frac{0.91527878λ^2}{λ^2-109.074599}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.27e-05 7.36e-09 -1.75e-13 4.58e-07 2.54e-10 0.183 nd: 1.619990 Vd: 63.763831 glass_code: 620638 density: 3.69 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.05e-05 K-1 - temperature_range: 20 300 ℃ coefficient: 1.28e-05 K-1 dPgF: 0.0062
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets