Optical constants of CDGM - ZLAF (Dense lanthanum flint)
H-ZLAF71AGT
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.54172779λ^2}{λ^2-131.963779}+\frac{2.03469901λ^2}{λ^2-0.0125481283}+\frac{0.264811834λ^2}{λ^2-0.055979471}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.47e-06 1.75e-08 -1.77e-11 6.76e-07 4.45e-10 0.301 nd: 1.850260 Vd: 32.216801 glass_code: 850322 density: 4.42 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.2e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.2e-06 K-1 dPgF: 0.0029 climatic_resistance: 1.0
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets