Optical constants of CDGM - ZLAF (Dense lanthanum flint)
H-ZLAF68B
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.43418261-0.0106199538λ^{2}+0.0400046303λ^{-2}-0.000637942235λ^{-4}+0.000216353029λ^{-6}-8.49876445\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.45e-07 1.47e-08 -7.21e-11 7.69e-07 2.19e-10 0.208 nd: 1.883004 Vd: 40.806875 glass_code: 883408 density: 5.53 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.4e-06 K-1 dPgF: -0.0067 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)