Optical constants of CDGM - ZLAF (Dense lanthanum flint)
H-ZLAF53BGT
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.302813825λ^2}{λ^2-0.04559202}+\frac{1.25522353λ^2}{λ^2-99.9412194}+\frac{1.95575794λ^2}{λ^2-0.010816711}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 9.87e-06 1.65e-08 -3.22e-11 8.9e-07 1.12e-09 0.243 nd: 1.834000 Vd: 37.210555 glass_code: 834372 glass_status: standard density: 4.54 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5.9e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.2e-06 K-1 dPgF: -0.004 climatic_resistance: 1.0
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets