Optical constants of CDGM - ZLAF (Dense lanthanum flint)
D-ZLAF85LS-25
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.70152719λ^2}{λ^2-0.00796295658}+\frac{0.633298236λ^2}{λ^2-0.0320099725}+\frac{1.43191921λ^2}{λ^2-110.67927}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.853440 Vd: 40.557917 glass_code: 853406 density: 5.29 g/cm3 thermal_expansion: - temperature_range: 20 300 ℃ coefficient: 8.1e-06 K-1 dPgF: -0.008
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets