Optical constants of CDGM - ZLAF (Dense lanthanum flint)
D-ZLAF85LS
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.638690484λ^2}{λ^2-0.0319257637}+\frac{1.69998504λ^2}{λ^2-0.00791790668}+\frac{1.45547394λ^2}{λ^2-112.179157}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.854500 Vd: 40.593546 glass_code: 855406 density: 5.29 g/cm3 thermal_expansion: - temperature_range: 20 300 ℃ coefficient: 8.1e-06 K-1 dPgF: -0.008
Comments
anneal rate:4℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets