Optical constants of CDGM - ZLAF (Dense lanthanum flint)
D-ZLAF85LN
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.92017081λ^2}{λ^2-0.00961912018}+\frac{0.386379034λ^2}{λ^2-0.0389567822}+\frac{1.291166λ^2}{λ^2-97.9773368}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.18e-06 1.74e-08 -3.81e-11 8.61e-07 5.26e-10 0.215 nd: 1.845580 Vd: 40.094322 glass_code: 846401 density: 4.96 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.2e-06 K-1 dPgF: -0.006 climatic_resistance: 1.0
Comments
anneal rate:4℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)