Optical constants of CDGM - ZLAF (Dense lanthanum flint)
D-ZLAF61-25
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.384732155λ^2}{λ^2-0.0355326885}+\frac{1.8424092λ^2}{λ^2-0.00916902591}+\frac{1.21280764λ^2}{λ^2-95.9091697}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.38e-06 1.46e-08 -1.77e-11 7.39e-07 6.32e-10 0.229 nd: 1.821310 Vd: 42.674895 glass_code: 821427 density: 4.92 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.5e-06 K-1 dPgF: -0.0068 climatic_resistance: 1.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)