Optical constants of CDGM - ZK (Dense crown)
H-ZK7
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.56229558-0.0108844706λ^{2}+0.0140997791λ^{-2}+0.000379257039λ^{-4}-2.41612681\text{×}10^{-05}λ^{-6}+1.41616214\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -5.31e-07 1.64e-08 -6.04e-11 3.53e-07 -1.4e-10 0.23 nd: 1.613095 Vd: 60.614383 glass_code: 613606 density: 3.51 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.1e-06 K-1 - temperature_range: 20 300 °C coefficient: 8e-06 K-1 dPgF: -0.0041 climatic_resistance: 4.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)