Optical constants of CDGM - ZK (Dense crown)
H-ZK5
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.54498193-0.00576275042λ^{2}+0.0196014743λ^{-2}-0.000812786508λ^{-4}+0.000138354802λ^{-6}-6.16579204\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.46e-06 1.21e-08 1.31e-11 5.78e-07 6.03e-10 0.17 nd: 1.611173 Vd: 55.812649 glass_code: 611558 density: 3.58 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.9e-06 K-1 dPgF: -0.005 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)