RefractiveIndex.INFO

Refractive index database


Shelf

Book

Page

Optical constants of CDGM - ZK (Dense crown)
H-ZK21

Wavelength: µm
 (0.300 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.894248925λ^2}{λ^2-0.00384521718}+\frac{0.696413489λ^2}{λ^2-0.0174130132}+\frac{1.07122355λ^2}{λ^2-102.205952}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: 8.71e-07 1.71e-08 -8.72e-11 4.27e-07 -7.8e-10 0.222
nd: 1.622990
Vd: 58.120667
glass_code: 623581
glass_status: standard
density: 3.56 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 6.2e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 7.5e-06 K-1
dPgF: -0.0024
climatic_resistance: 1.0

References

CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

CDGM Glass Co., Ltd.

CDGM Glass Co., Ltd. is a leading optical glass supplier in China with a worldwile distribution network.

External links


Glass

External links