Optical constants of CDGM - ZK (Dense crown)
H-ZK20
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.56416217-0.00663710078λ^{2}+0.0191195924λ^{-2}-0.000520583562λ^{-4}+0.000117796641λ^{-6}-5.72026705\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.96e-07 3.18e-08 4.78e-11 5.07e-07 -2.17e-09 0.255 nd: 1.617203 Vd: 53.928400 glass_code: 617539 density: 3.66 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 9e-06 K-1 dPgF: -0.0001
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)