Optical constants of CDGM - ZK (Dense crown)
H-ZK2
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.427442699λ^2}{λ^2-0.0191755139}+\frac{0.907023646λ^2}{λ^2-94.6355569}+\frac{1.04012009λ^2}{λ^2-0.00552619449}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.23e-06 2.61e-08 -7.02e-11 4.76e-07 -6.76e-10 0.184 nd: 1.583130 Vd: 59.460082 glass_code: 583595 density: 3.24 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.1e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 7.8e-06 K-1 dPgF: -0.0016 climatic_resistance: 2.0
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)