Optical constants of CDGM - ZK (Dense crown)
D-ZK3L-25
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.636443631λ^2}{λ^2-0.0021737174}+\frac{0.856921557λ^2}{λ^2-0.0144861653}+\frac{1.23247717λ^2}{λ^2-107.585666}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.09e-06 1.33e-08 5.99e-11 4.94e-07 2.85e-10 0.176 nd: 1.590900 Vd: 60.618517 glass_code: 591606 density: 2.84 g/cm3 thermal_expansion: - temperature_range: 20 300 ℃ coefficient: 9.2e-06 K-1 dPgF: -0.0046
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)