Optical constants of CDGM - ZK (Dense crown)
D-ZK2L
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.512521894λ^2}{λ^2-0.0176943616}+\frac{0.967402158λ^2}{λ^2-0.00510795325}+\frac{1.12488967λ^2}{λ^2-109.10377}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.09e-06 1.37e-08 -3.16e-11 4.84e-07 4.03e-10 0.189 nd: 1.587000 Vd: 59.600321 glass_code: 587596 density: 2.99 g/cm3 thermal_expansion: - temperature_range: 20 300 ℃ coefficient: 9e-06 K-1 dPgF: -0.0033
Comments
anneal rate:4℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets