Optical constants of CDGM - ZK (Dense crown)
D-ZK21-25
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.08777542λ^2}{λ^2-0.0143531981}+\frac{0.505694645λ^2}{λ^2+0.000448862561}+\frac{1.31533152λ^2}{λ^2-104.063333}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.26e-06 1.53e-08 -2.43e-11 4.86e-07 2.51e-10 0.199 nd: 1.623460 Vd: 58.115078 glass_code: 623581 density: 2.99 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.1e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.4e-06 K-1 dPgF: -0.0066 climatic_resistance: 1.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)