Optical constants of CDGM - ZK (Dense crown)
D-ZK2-25
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.1044946λ^2}{λ^2-0.0062094807}+\frac{0.36094124λ^2}{λ^2-0.0196844329}+\frac{1.01208343λ^2}{λ^2-101.038646}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2e-06 1.15e-08 4.47e-11 6.34e-07 6.43e-10 0.089 nd: 1.582410 Vd: 59.308255 glass_code: 582593 density: 2.96 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.2e-06 K-1 dPgF: -0.0035 climatic_resistance: 2.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)