Optical constants of CDGM - ZF (Dense flint)
ZF8
Wavelength:
µm
(0.330 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.6567173-0.0091117044λ^{2}+0.025815197λ^{-2}+0.0011203564λ^{-4}-4.1066817\text{×}10^{-05}λ^{-6}+6.9242011\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.654460 Vd: 33.651201 glass_code: 654337 glass_status: preferred density: 3.91 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8.9e-06 K-1 dPgF: -0.0001 climatic_resistance: 1.0
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets