$$n^2=3.1221966-0.010649791λ^{2}+0.042191871λ^{-2}+0.002893766λ^{-4}-0.00016523594λ^{-6}+2.329181\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.806277 Vd: 25.380144 glass_code: 806254 density: 5.19 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 9e-06 K-1 dPgF: 0.0073 climatic_resistance: 1.0
References