Optical constants of CDGM - ZF (Dense flint)
ZF6
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.96285995-0.0104077823λ^{2}+0.0356441238λ^{-2}+0.00245699205λ^{-4}-0.000149615893λ^{-6}+1.77827751\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.755205 Vd: 27.546239 glass_code: 755275 density: 4.78 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.4e-06 K-1 dPgF: 0.002 climatic_resistance: 1.0
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets