Optical constants of CDGM - ZF (Dense flint)
ZF51
Wavelength:
µm
(0.360 – 2.400)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.06187076-0.0138733563λ^{2}+0.032985222λ^{-2}+0.00507141578λ^{-4}-0.000538606629λ^{-6}+4.36089245\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.8e-06 2.76e-08 -6.03e-11 1.6e-06 1.02e-09 0.279 nd: 1.784701 Vd: 26.075871 glass_code: 785261 density: 4.99 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.2e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.02e-05 K-1 dPgF: 0.0052 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)