Optical constants of CDGM - ZF (Dense flint)
ZF4
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.89234898-0.0179339416λ^{2}+0.0230094722λ^{-2}+0.00563906172λ^{-4}-0.000698154951λ^{-6}+5.25289979\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -3.94e-06 1.2e-08 -6.11e-11 8.57e-07 1.51e-09 0.293 nd: 1.728251 Vd: 28.323900 glass_code: 728283 glass_status: preferred density: 4.51 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 1.11e-05 K-1 dPgF: 0.0064 climatic_resistance: 1.0
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets
Data
INFO
SF10 optical glass
SF10 is a popular optical glass. Most glass makers produce this or very similar glass under slightly different names.SF10 and similar glasses produced by different makers
Maker | Glass |
---|---|
Schott | N-SF10 |
Hikari | E-SF10 |
HOYA | E-FD10 |
Sumita | K-SFLD10 |
CDGM | ZF4 |