Optical constants of CDGM - ZF (Dense flint)
ZF3
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.84758519-0.0105088281λ^{2}+0.0309450925λ^{-2}+0.00213696398λ^{-4}-0.00013104012λ^{-6}+1.42428874\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.61e-06 2.44e-08 -3.11e-10 1.38e-06 1.2e-09 0.261 nd: 1.717365 Vd: 29.510385 glass_code: 717295 density: 4.46 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.5e-06 K-1 dPgF: 0.0012 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)