Optical constants of CDGM - ZF (Dense flint)
H-ZF71
Wavelength:
µm
(0.370 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.406804868λ^2}{λ^2-0.064515213}+\frac{1.70831097λ^2}{λ^2-0.0127703237}+\frac{2.36137303λ^2}{λ^2-163.275585}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -9.66e-06 1.15e-08 -5.06e-11 9.75e-07 1.26e-09 0.313 nd: 1.808100 Vd: 22.698087 glass_code: 808227 density: 3.3 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.3e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 1.05e-05 K-1 dPgF: 0.0224 climatic_resistance: 1.0
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets