Optical constants of CDGM - ZF (Dense flint)
H-ZF52A

Wavelength: µm
 (0.370 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=3.2506862-0.0133942217λ^{2}+0.0483625913λ^{-2}+0.00314442751λ^{-4}-0.000197073674λ^{-6}+3.47645679\text{×}10^{-05}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -6.9e-06 1.71e-08 -4.57e-11 1.16e-06 8.99e-10 0.285
nd: 1.846670
Vd: 23.791236
glass_code: 847238
glass_status: preferred
density: 3.52 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 8.4e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.04e-05 K-1
dPgF: 0.0151
climatic_resistance: 1.0

References

CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

CDGM Glass Co., Ltd.

CDGM Glass Co., Ltd. is a leading optical glass supplier in China with a worldwile distribution network.

External links


Glass

External links