Optical constants of CDGM - ZF (Dense flint)
H-ZF50

Wavelength: µm
 (0.365 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.38419227λ^2}{λ^2-121.210226}+\frac{0.216862697λ^2}{λ^2-0.0642534343}+\frac{1.69855074λ^2}{λ^2-0.0135195855}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -4.21e-06 1.99e-08 -3e-11 8.92e-07 3.64e-10 0.294
nd: 1.740770
Vd: 27.760063
glass_code: 741278
density: 3.1 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 9.5e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.13e-05 K-1
dPgF: 0.0109
climatic_resistance: 1.0

References

CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

CDGM Glass Co., Ltd.

CDGM Glass Co., Ltd. is a leading optical glass supplier in China with a worldwile distribution network.