Optical constants of CDGM - ZF (Dense flint)
H-ZF4AGT

Wavelength: µm
 (0.365 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.67238093λ^2}{λ^2-0.0133653851}+\frac{1.34134437λ^2}{λ^2-122.464022}+\frac{0.204305471λ^2}{λ^2-0.0641192325}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -5.36e-06 1.47e-08 -3.86e-11 1.02e-06 8.24e-10 0.276
nd: 1.728250
Vd: 28.318797
glass_code: 728283
glass_status: standard
density: 3.05 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 9.3e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.12e-05 K-1
dPgF: 0.0107
climatic_resistance: 1.0

References

CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

CDGM Glass Co., Ltd.

CDGM Glass Co., Ltd. is a leading optical glass supplier in China with a worldwile distribution network.

External links


Glass

External links