Optical constants of CDGM - ZF (Dense flint)
D-ZF93-25
Wavelength:
µm
(0.400 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.4330228λ^2}{λ^2-101.185435}+\frac{2.13630545λ^2}{λ^2-0.0138161232}+\frac{0.630184037λ^2}{λ^2-0.065857845}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.28e-05 3.34e-08 -1.53e-10 2.75e-06 2.52e-09 0.299 nd: 1.999800 Vd: 20.686444 density: 6.11 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.8e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.4e-06 K-1 dPgF: 0.0283 climatic_resistance: 1.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)