Optical constants of CDGM - ZF (Dense flint)
D-ZF93
Wavelength:
µm
(0.400 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.51323628λ^2}{λ^2-106.262695}+\frac{2.16740096λ^2}{λ^2-0.014231857}+\frac{0.606108042λ^2}{λ^2-0.0666586743}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.28e-05 3.34e-08 -1.53e-10 2.75e-06 2.52e-09 0.299 nd: 2.001700 Vd: 20.700195 density: 6.11 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.8e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.4e-06 K-1 dPgF: 0.0285 climatic_resistance: 1.0
Comments
anneal rate:4℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets