Optical constants of CDGM - ZF (Dense flint)
D-ZF10-25
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.39531577λ^2}{λ^2-134.661574}+\frac{0.180389834λ^2}{λ^2-0.0604305431}+\frac{1.57395389λ^2}{λ^2-0.0122657049}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -5.76e-06 6.62e-09 -3.57e-11 9.8e-07 1.12e-09 0.261 nd: 1.687310 Vd: 31.183804 glass_code: 687312 density: 2.84 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1e-05 K-1 - temperature_range: 20 300 ℃ coefficient: 1.29e-05 K-1 dPgF: 0.0067 climatic_resistance: 1.0
Comments
anneal rate:25℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)