Optical constants of CDGM - ZBAF (Dense barium flint)
ZBAF17
Wavelength:
µm
(0.350 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.7114815-0.0083031047λ^{2}+0.023733195λ^{-2}+0.00028197729λ^{-4}+3.9409899\text{×}10^{-05}λ^{-6}+7.1756265\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.29e-08 1.54e-08 -1.58e-11 7.94e-07 1.05e-09 0.24 nd: 1.667554 Vd: 41.957211 glass_code: 668419 density: 3.8 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.1e-06 K-1 dPgF: -0.0014 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)