Optical constants of CDGM - ZBAF (Dense barium flint)
H-ZBAF1
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.57943-0.00757753047λ^{2}+0.0201786053λ^{-2}-0.000845832798λ^{-4}+0.000178126935λ^{-6}-9.19232657\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.71e-06 2.12e-08 -1.14e-10 4.62e-07 6.87e-11 0.246 nd: 1.622297 Vd: 53.199535 glass_code: 622532 density: 3.57 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.2e-06 K-1 dPgF: 0.0011
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)