Optical constants of CDGM - TF (Special flint)
H-TF3L
Wavelength:
µm
(0.330 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5493446-0.012566087λ^{2}+0.018232175λ^{-2}+0.00067809743λ^{-4}-2.8500371\text{×}10^{-05}λ^{-6}+3.2560812\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.613395 Vd: 44.166804 glass_code: 613441 density: 2.8 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.7e-06 K-1 dPgF: -0.0083 climatic_resistance: 1.0
References
CDGM Zemax catalog 2017-09 (obtained from http://www.cdgmgd.com)