Optical constants of CDGM - QK (Light crown)
D-QK3L
Wavelength:
µm
(0.280 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.601737491λ^2}{λ^2-0.012574974}+\frac{0.858737004λ^2}{λ^2-92.3325663}+\frac{0.586761501λ^2}{λ^2-0.002687509}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -9.26e-06 1.71e-08 -1.54e-11 3.26e-07 5.95e-10 0.187 nd: 1.487490 Vd: 70.440487 glass_code: 487704 density: 2.43 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.1e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 1.01e-05 K-1 dPgF: 0.0035 climatic_resistance: 2.0
Comments
anneal rate:4℃/h
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets