Optical constants of CDGM - QF (Light flint)
H-QF8

Wavelength: µm
 (0.340 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.127874264λ^2}{λ^2-0.0424546034}+\frac{1.20201357λ^2}{λ^2-0.00811385854}+\frac{0.92946936λ^2}{λ^2-109.832978}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 ℃
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -2.28e-06 1.48e-08 -8.66e-11 5.08e-07 1.15e-10 0.282
nd: 1.540720
Vd: 47.230007
glass_code: 541472
density: 2.54 g/cm3
thermal_expansion:
  - temperature_range: -30 70 ℃
    coefficient: 9.6e-06 K-1
  - temperature_range: 20 300 ℃
    coefficient: 1.13e-05 K-1
dPgF: 0.0002
climatic_resistance: 2.0

References

CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)
See also CDGM optical glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

CDGM Glass Co., Ltd.

CDGM Glass Co., Ltd. is a leading optical glass supplier in China with a worldwile distribution network.

External links


Glass

External links