Optical constants of CDGM - QF (Light flint)
H-QF50
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.29450546λ^2}{λ^2-0.00894503808}+\frac{0.150752291λ^2}{λ^2-0.0483713581}+\frac{1.08698065λ^2}{λ^2-113.959763}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.05e-07 2.23e-09 5.39e-11 5.36e-07 1.83e-09 0.288 nd: 1.581440 Vd: 40.888972 glass_code: 581409 density: 2.6 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.7e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.9e-06 K-1 dPgF: 0.0013
References
CDGM Zemax catalog 2022-06 (obtained from http://www.cdgmgd.com)